Harbor Freight Company founder Eric Smidt announced the company had discovered a new welding defect in its three-ton jack stands significant enough to warrant a voluntary safety recall. These jack stands that are subject to the latest recall were supposed to be the safe alternatives to the faulty, previously recalled jack stands.

In May, Harbor Freight issued a recall of 454,000 jack stands manufactured between 2013 and 2019 over fears that the products could collapse and cause serious injury or death.

Nearly two months after the original recall, it became clear that a new problem was present and that it affected even more jack stands sold by Harbor Freight.

Harbor Freight said that it had “identified a welding defect” in some of its three-ton Pittsburgh-branded jack stands and have since added the units to its recall. Engineers also investigated other jack stands that it sells and were not able to identify any defects, however as a precautionary measure, the retailer is offering to exchange any of its jack stands for customers who have safety concerns.

Customers should check the item number on their jack stands and use the Harbor Freight website to verify that their product is included on the recall.

Depending on the specific model, customers can exchange the units for a cash refund between $24.99 and $11.99, or store credit of $29.99 and $143.99.

Share

Litigation Updates

Class Action Lawsuit Alleges Harbor Freight Jack Stand Can Collapse While Under Loads

September 20, 2020

September 20, 2020

Class Action Lawsuit Alleges Harbor Freight Jack Stand Can Collapse While Under Loads

Harbor Freight Jack Stands Recalled Again Over Weld Defects

July 7, 2020

July 7, 2020

Harbor Freight Jack Stands Recalled Again Over Weld Defects

Harbor Freight Customer’s Replacement Jack Stands are Also Faulty

June 12, 2020

June 12, 2020

Harbor Freight Customer’s Replacement Jack Stands are Also Faulty

CLIENT REVIEWS

quotation
Lisa

From the moment I met them, it felt like a weight lifted – TorHoerman Law was confident, ready to fight, and truly cared about me as a person.

quotation
Jane

Rear-ended on my way to work, I ended up a patient in my own ER – TorHoerman Law took over the insurance nightmare so I could focus on getting better.

quotation
TJ

After months of chiropractic bills from an accident that wasn’t my fault, TorHoerman Law got involved and made the whole process easy – they treat you like family, not a number.

quotation
Richard "Doc" Holliday

After a hit-and-run left me with a shattered leg and no idea where to turn – TorHoerman Law took over everything, got me every dollar available, and made me feel like family.

quotation
Trish Jones

I have had many speed bumps to get over on information needed to file my claim that has had me stressing out several times, but once I have gotten in touch with TorHoerman Law I always come out with most of my problems handled. Nikki has been very much helpful in aiding me with my complaint and never lets me go feeling like I’m clueless as to what to do next. She listens and responds very efficiently and with very positive attitude and that’s always helpful. Thanks TorHoerman Law for your advice and support I appreciate all y’all have done for me.

quotation
Amari Raglin

I was in a car accident and went to the Personal Injury Team at TorHoerman Law. I met with Kristie Stephens and she was awesome, keeping me informed of what was going on, what to expect and not to hesitate to call if I need any questions answered. The staff I came in contact over the phone was Kristine Stephens, and she guided me through the whole process. I suggest the Personal Injury Team at TorHoerman Law for anybody that needs help with legal action.

quotation
Tom Lewis

TorHoerman Law was responsible for handling a medical case for our family. I was extremely impressed with their professionalism and ability to react quickly. They also did a nice job keeping us updated with the case throughout the process. This was the first time experiencing a situation like this and Tor Hoerman law did an excellent job from start to finish.

quotation
Dave Woodley

All of my questions were answered quickly and in a way I could understand. Steve and the entire staff were friendly and professional.